AISI 4340H Steel, normalized 870°C (1600°F)
Subcategory: Low Alloy Steel; AISI 4000 Series Steel; Medium Carbon Steel; Metal
Close Analogs: AISI 4340, AISI E4340, AISI E4340 H
Key Words: alloy steels, UNS H43406, ASTM A304, SAE J1268, DIN 1.6565, IS 1570 40Ni2Cr1Mo28, IS 1570 40NiCr1Mo15
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Izod Impact
- Machinability
- Shear Modulus
- Electrical Resistivity
- Electrical Resistivity at Elevated Temperature
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|