AISI E4340 Steel, oil quenched 800°C (1470°F), 595°C (1100°F) temper, 25 mm round
Subcategory: Low Alloy Steel; AISI 4000 Series Steel; Medium Carbon Steel; Metal
Close Analogs: AISI 4340, AISI 4340 H, AISI E4340 H
Key Words: alloy steels, UNS G43406, ASTM A304, ASTM A331, ASTM A505, ASTM A519
Material Notes: Post oil quenched hardness: 57 HRC - surface, 57 HRC - 1/2 radius, 56 HRC - center.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- Electrical Resistivity at Elevated Temperature
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|