AISI E4340 H Steel, normalized, oil quenched and tempered
Subcategory: Low Alloy Steel; AISI 4000 Series Steel; Medium Carbon Steel; Metal
Close Analogs: AISI 4340, AISI 4340H, AISI E4359
Key Words: alloy steels, UNS H43406, ASTM A304, SAE J1268, DIN 1.6562
Material Notes: heat treatment and testing: normalized 940 - 955°C, oil quenched 830°C, 540°C temper. R.R. Moore rotating beam fatigue specimens with a min. diam. of 5.84 mm; 45°, 0.25 mm root radius notch, 0.51 mm deep.
| Available Properties |
- Density
- Hardness, Knoop
- Hardness, Rockwell C
- Hardness, Vickers
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- Electrical Resistivity at Elevated Temperature
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|