AISI 4427 Steel, heat treated in 13.7 mm rounds, reheated to 805°C (1480°F), 150°C (300°F) temper
Subcategory: Low Alloy Steel; AISI 4000 Series Steel; Low Carbon Steel; Metal
Key Words: alloy steels, UNS G44270, ASTM A519, SAE J404, SAE J412, SAE J770
Material Notes: Heat treatment: Normalized at 925°C (1700°F) in 32 mm rounds, machined to 13.7 mm rounds, pseudo carburized at 925°C (1700°F) for 8 hrs., box cooled to RT, reheated to 805°C (1480°F), oil quenched, 150°C (300°F) temper, tested in 12.8 mm rounds.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|