AISI 4718H Steel, psueudocarburized, reheated to 850°C (1560°F) and oil quenched, 150°C (300°F) temper, 13.7 mm round
Subcategory: Low Alloy Steel; AISI 4000 Series Steel; Low Carbon Steel; Metal
Key Words: alloy steels, UNS H47180, ASTM A304, SAE J1268, DIN 1.6755
Material Notes: Full heat treatment: normalized at 925°C (1700°F), machined to 13.7 mm (1 in.), pseudocarburized at 925°C (1700°F) for 8 hours, box cooled to RT, reheated to 850°C (1560°F), 150°C (300°F) temper, machined and tested in 12.8 mm (0.505 in.) rounds
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|