AISI 4815 Steel, pseudocarburized, reheated to 800°C (1470°F) and oil quenched, 150°C (300°F) temper, 25 mm (1 in.) round
Subcategory: Low Alloy Steel; AISI 4000 Series Steel; Low Carbon Steel; Metal
Close Analogs: AISI 4815H
Key Words: UNS G48150, ASTM A322, ASTM A331, ASTM A505, SAE J404, SAE J412, SAE J770, low carbon steels
Material Notes: Normalized 925°C (1700°F) in 32mm rounds, machined to 25 mm rounds, pseudocarburized at 925°C (1700°F) for 8 h., box cooled to RT, reheated to 800°C (1470°F), oil quenched, 150°C (300°F) temper, machined and tested in 12.8mm rounds.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- Electrical Resistivity at Elevated Temperature
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|