AISI 4820 Steel, direct quenched from pot, tempered 150°C (300°F), 0.99 mm case depth
Subcategory: Low Alloy Steel; AISI 4000 Series Steel; Low Carbon Steel; Metal
Close Analogs: AISI 4820H
Key Words: SAE 770, low carbon steels, UNS G48200, ASTM A322, ASTM A331, ASTM A505, ASTM A519, ASTM A535, SAE J404, SAE J414,
Material Notes: Carburized at 925°C (1700°F) for 8 hrs., oil quenched, 150°C (300°F) temper. 0.99mm case depth. Recommended practice for max. case hardness
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|