AISI 5140H Steel, oil quenched 845°C (1550°F), 540°C (1000°F) temper, 25 mm (1 in.) round
Subcategory: Low Alloy Steel; AISI 5000 Series Steel; Medium Carbon Steel; Metal
Close Analogs: AISI 5140
Key Words: UNS H51400, ASTM A304, SAE J1268, DIN 1.7006, AFNOR 42 C 2 (Fr), AFNOR 45 C 2 (Fr)
Material Notes: Oil quenched from 845°C, 540°C temper, 25 mm round. Post oil quenched hardness 53 HRC surface, 48 HRC half-radius, 45 HRC center
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- Electrical Resistivity at Elevated Temperature
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Specific Heat Capacity at Elevated Temperature
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|