AISI 6150 Steel, oil quenched 845°C (1550°F), 650°C (1200°F) temper, 13 mm (0.5 in.) round
Subcategory: Low Alloy Steel; AISI 6000 Series Steel; Medium Carbon Steel; Metal
Close Analogs: AISI 6150H
Key Words: AFNOR 50 CV 4 (Fr), UNI 50 CrV 4, JIS SUP 10, SS14 2230 (Sweden), B.S. 735 A 50, B.S. En. 47, ASTM A505, MIL-SPEC MIL-S-8503, SAE J404, SAE J412, SAE J770, DIN 1.8159, UNS G51500, AMS 6448, AMS 6450, AMS 7301, ASTM A231, ASTM A322, ASTM A331
Material Notes: Oil quenched from 845°C, 650°C (1200°F) temper, 13 mm round, post oil quenched hardness 61 HRC surface, 60 HRC half-radius, 60 HRC center. Applications: Automotive leaf springs.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|