AISI 6150H Steel, oil quenched 845°C (1550°F), 650°C (1200°F) temper, 50 mm (2 in.) round
Subcategory: Low Alloy Steel; AISI 6000 Series Steel; Medium Carbon Steel; Metal
Close Analogs: AISI 6150
Key Words: B.S. 735 A 50, UNI 50 CrV 4, JIS SUP 10, SS14 2230 (Sweden), B.S. En 47, UNS H61500, ASTM A304, SAE J1268, DIN 1.8159, AFNOR 50 CV 4 (Fr)
Material Notes: Oil quenched from 845°C, 650°C (1200°F) temper, 50 mm round, post oil quenched hardness 54 HRC surface, 47 HRC half-radius, 44 HRC center. Applications: Automotive leaf springs.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|