AISI 8617 Steel, double quenched, 150°C (300°F) temper
Subcategory: Low Alloy Steel; AISI 8000 Series Steel; Low Carbon Steel; Metal
Close Analogs: AISI 8617H
Key Words: DIN 1.6523, AFNOR 20 NCD 2 (Fr), AFNOR 22 NCD 2 (Fr), UNI NiCrMo 2, JIS SNCM 21 H, JIS SNCM 21, B.S. 805 H 20, B.S. 805 M 20, UNS G86170, ASTM A322, ASTM A331, ASTM A505, AMS 6272, SAE J404, SAE J770
Material Notes: Normalized 925°C (1700°F) in 32 mm rounds, machined to 25 or 13.7 mm rounds, pseudocarburized at 925°C (1700°F) for 8 hours, box cooled to room temperature, reheated to 855°C (1570°F), oil quenched, reheated to 800°C (1470°F), oil quenched, 150°C (300°F) temper, tested in 12.8 mm rounds. Post oil quenched hardness 25 mm: 302 HB at 7/8 radius, 265 HB at half-radius, 258 HB at center; 50 mm: 235 HB at 7/8 radius, 215 HB at half-radius, 207 HB at center
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|