AISI 8620 Steel, quenched from 900°C (1650°F), tempered at 425°C (800°F), Low temp impact properties
Subcategory: Low Alloy Steel; AISI 8000 Series Steel; Low Carbon Steel; Metal
Close Analogs: AISI 8620H
Key Words: AFNOR 22 NCD 2, UNI 20 NiCrMo 2, JIS SNCM 21 H, JIS SNCM 21, B.S. 805 H 20 (UK), B.S. 805 M 20 (UK), MIL SPEC MIL-S-16794, SAE J404, SAE J770, DIN 1.6523, AFNOR 20 NCD 2 (France), UNS G86200, AMS 6274, AMS 6276, AMS 6277, ASTM A322, ASTM A331, ASTM A505, ASTM A523
Material Notes: Transition temperature: -29°C (50% Brittle)
| Available Properties |
- Density
- Hardness, Knoop
- Hardness, Rockwell C
- Hardness, Vickers
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Izod Impact
- Machinability
- Shear Modulus
- Electrical Resistivity
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|