AISI 8620H Steel, quenched from carburizing box, 25 mm (1 in.) round
Subcategory: Low Alloy Steel; AISI 8000 Series Steel; Low Carbon Steel; Metal
Close Analogs: AISI 8620
Key Words: AFNOR 22 NCD 2, UNI 20 NiCrMo 2, JIS SNCM 21 H, JIS SNCM 21, B.S. 805 H 20 (UK), B.S. 805 M 20 (UK), UNS H86200,ASTM A304, SAEJ1268, DIN 1.6523, AFNOR 20 NCD 2 (France)
Material Notes: Quenched from carburizing box: carburized at 925°C (1700°F) for 8 hrs., oil quenched, 150°C. Tested at center
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|