AISI 8622 Steel, heat treated, machined to 13.7 mm rounds, pseudocarburized, 775°C (1430°F) reheat, 150°C (300°F) temper
Subcategory: Low Alloy Steel; AISI 8000 Series Steel; Low Carbon Steel; Metal
Close Analogs: AISI 8622H
Key Words: B.S. 805 A 20, UNS G86220, ASTM A322, ASTM A331, SAE J404, SAE J770, DIN 1.6543, ASTM A304, SAE J1268, DIN 1.6543, B.S. 805 A 20
Material Notes: Normalize 925°C (1700°F) in 32 mm rounds, machine to 13.7 mm rounds, pseudocarburize at 925°C (1700°F) for 8 hours, box cooled to room temperature, 775°C (1430°F) reheat, oil quench, 150°C (300°F) temper, tested in 12.8 mm rounds
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|