AISI 86B45 Steel, normalized at 870°C (1600°F), oil quenched 845°C (1550°F), 540°C (1000°F) temper, 25 mm diam.
Subcategory: Low Alloy Steel; AISI 8000 Series Steel; Medium Carbon Steel; Metal
Close Analogs: AISI 8645, AISI 8645H, AISI 86B45H
Key Words: UNS G86451, ASTM A519, SAE J404, SAE J412, SAE J770
Material Notes: Test specimen was a 12.8 mm (0.505 in) round
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Bulk Modulus
- Shear Modulus
|
|
|
|