AISI 8822 Steel, normalized, machined to 13.7 mm rounds, pseudocarburized, 775°C (1430°F) reheat, 150°C (300°F) temper
Subcategory: Low Alloy Steel; AISI 8000 Series Steel; Low Carbon Steel; Metal
Close Analogs: AISI 8822H
Key Words: B.S. 805 A 20, UNS G88220, ASTM A322, ASTM A331, ASTM A519, SAE J404, SAE J770, DIN 1.6543
Material Notes: Normalized at 925°C in 32 mm rounds, machined to 13.7 mm rounds, 925°C pseudocarburized for 8 hours, box cooled to room temperature, 775°C reheat, oil quench, 150°C temper, tested in 12.8 mm rounds
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|