AISI 9255 Steel, oil quenched from 885°C (1625°F), 595°C (1100°F) temper, 25 mm (1 in.) round
Subcategory: Low Alloy Steel; AISI 9000 Series Steel; Medium Carbon Steel; Metal
Key Words: AFNOR 55 S 7, UNI 55 Si 8, SS14 2085 (Sweden), B.S. 250 A 53, UNS G92550, ASTM A322, ASTM A519, SAE J404, SAE J412, SAE J770, DIN 1.0904
Material Notes: Post oil quenched hardness 57 HRC surface, 55 HRC half-radius,48 HRC center
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|