AISI 9260 Steel
Subcategory: Low Alloy Steel; AISI 9000 Series Steel; High Carbon Steel; Metal
Close Analogs: AISI 9260H
Key Words: B.S. 250 A 58, SAE J404, SAE J412, SAE J770, DIN 1.0909, AFNOR 60 SC 7, AFNOR 61 SC 7 (France), UNS G92600, ASTM A29, ASTM A59, ASTM A322, ASTM A331, ASTM A505, ASTM A519
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|