AISI E9310 Steel, mock carburized, 790°C (1450°F) reheat, 230°C (450°F) temper, 100 mm (4 in.) round
Subcategory: Low Alloy Steel; AISI 9000 Series Steel; Low Carbon Steel; Metal
Close Analogs: AISI E9310H
Key Words: SAE J770, UNS G93106, AMS 6260F, AMS 6265B, ASTM A322, ASTM A519, ASTM A711, SAE J404
Material Notes: Mock carburized at 925°C for 8 hours, 790°C reheat, oil quenched, 230°C temper, 100 mm round. Post oil quenched hardness 31 HRC surface, 30 HRC half-radius, 29 HRC center
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|