AISI E9310H Steel, normalized, machined to 25 mm (1 in.) rounds, pseudocarburized, 800°C (1470°F) reheat, 150°C (300°F) temper
Subcategory: Low Alloy Steel; AISI 9000 Series Steel; Low Carbon Steel; Metal
Close Analogs: AISI E9310
Key Words: UNS H93100, ASTM A304, SAE J1268
Material Notes: Normalized at 925°C in 32 mm rounds, machined to 25 mm rounds, pseudocarburized at 925°C for 8 hours, box cooled to room temperature, 800°C reheat, oil quenched, 150°C temper, tested in 12.8 mm rounds
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|