AISI 94B17 Steel
Subcategory: Low Alloy Steel; AISI 9000 Series Steel; Low Carbon Steel; Metal
Close Analogs: AISI 94B17H
Key Words: UNS G94171, AMS 6275, ASTM A322, ASTM A331, ASTM A519, SAE J404, SAE J770
| Available Properties |
- Density
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|