AISI 9840 Steel, 595°C (1100°F) temper, 25 mm (1 in.) round
Subcategory: Low Alloy Steel; AISI 9000 Series Steel; Medium Carbon Steel; Metal
Key Words: UNS G98400, AMS 6342 C, ASTM A274, ASTM A322, ASTM A519, SAE J778, DIN 1.6511, UNI 38 NiCrMo 4, B.S. 816 M 40
Material Notes: Quenched, 540°C temper, 525°C nitride for 40 hours with 20-30% ammonia dissociation, hardness of 88 HR15N case hardness at 0.635-0.762 mm nitrided case depth
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|