Aluminum Alloys, General
Subcategory: Aluminum Alloy; Nonferrous Metal
Key Words: Aluminium Alloys, General; Al Alloys
Material Notes: These properties are typical of commercial aluminum alloys. Some properties, such as strength and hardness, vary too much for a reasonable generalization. See entries for individual alloys for more specific information. Aluminum 1199 is the highest purity (99.99% Al min.) in the database.
| Available Properties |
- Density
- Modulus of Elasticity
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- Heat of Fusion
- CTE, linear 20°C
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |