Aluminum 1350-H14
Subcategory: Aluminum Alloy; Nonferrous Metal; 1000 Series Aluminum
Close Analogs: Composition Notes: The aluminum content for unalloyed aluminum not made by a refining process is the difference between 100.00 percent and the sum of all other analyzed metallic elements present in amounts of 0.010 percent of more each, expressed to the second decimal before determining the sum. For alloys and unalloyed aluminum not made by a refining process, when the specified maximum limit is 0.XX, an observed value or a calculated value greater than 0.005 but less than 0.010% is rounded off and shown as " less than 0.01%". Composition information provided by the Aluminum Association and is not for design.
Key Words: Aluminium 1350-H14; Electrical Conductor Grade (EC); UNS A91350; NF A5/L (France); AA1350-H14, BS1E (UK); DIN E-Al99.5
Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.
| Available Properties |
- Density
- Hardness, Brinell
- Ultimate Tensile Strength
- Tensile Yield Strength
- Modulus of Elasticity
- Poissons Ratio
- Shear Modulus
- Shear Strength
- Electrical Resistivity
- Heat of Fusion
- CTE, linear 68°F
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Annealing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|