Aluminum 2319
Subcategory: Aluminum Alloy; Nonferrous Metal; 2000 Series Aluminum Alloy
Close Analogs: Composition Notes: 0.0008% max Be for welding electrode and filler wire only. Aluminum content reported is calculated as remainder. Composition information provided by the Aluminum Association and is not for design.
Key Words: UNS A92319; MIL-E-16053; QQ-R-566; Aluminium 2319; AA2319
Material Notes: Used for electrodes and filler wire when welding Aluminum 2219 Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.
| Available Properties |
- Density
- Modulus of Elasticity
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Annealing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|