|   Aluminum 6061-T6; 6061-T651  Subcategory: Aluminum Alloy; Nonferrous Metal; 6000 Series Aluminum Alloy Close Analogs:  Composition Notes: Aluminum content reported is calculated as remainder.
 Composition information provided by the Aluminum Association and is not for design.
 Key Words: al6061, UNS A96061; ISO AlMg1SiCu; Aluminium 6061-T6, AD-33 (Russia); AA6061-T6; 6061T6, UNS A96061; ISO AlMg1SiCu; Aluminium 6061-T651, AD-33 (Russia); AA6061-T651 Material Notes: Information provided by Alcoa, Starmet and the references.  General 6061 characteristics and uses: Excellent joining characteristics, good acceptance of applied coatings. Combines relatively high strength, good workability, and high resistance to corrosion; widely available.  The T8 and T9 tempers offer better chipping characteristics over the T6 temper.
 Applications: Aircraft fittings, camera lens mounts, couplings, marines fittings and hardware, electrical fittings and connectors, decorative or misc. hardware, hinge pins, magneto parts, brake pistons, hydraulic pistons, appliance fittings, valves and valve parts; bike frames. Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN. 
| | 
    | Available Properties |  
    | DensityHardness, BrinellHardness, KnoopHardness, Rockwell AHardness, Rockwell BHardness, VickersUltimate Tensile StrengthTensile Yield StrengthElongation at BreakModulus of ElasticityNotched Tensile StrengthUltimate Bearing StrengthBearing Yield StrengthPoissons RatioFatigue StrengthFracture ToughnessMachinabilityShear ModulusShear StrengthElectrical ResistivityCTE, linear 68°FCTE, linear 250°CSpecific Heat CapacityThermal ConductivityMelting PointSolidusLiquidusSolution TemperatureAging Temperature
 | 
 | 
 |  | | 
    | Property Data |  
    | 
    This page displays only the textof a material data sheet.
 
 To see MatWeb's complete data
 sheet for this material (including
 material property data, metal
 compositions, material suppliers,
 etc), please click the button below.
 |  
    |  | 
 | 
 | 
 |