Aluminum 6063-T6
Subcategory: Aluminum Alloy; Nonferrous Metal; 6000 Series Aluminum Alloy
Close Analogs: Composition Notes: Aluminum content reported is calculated as remainder. Composition information provided by the Aluminum Association and is not for design.
Key Words: UNS A96063; ISO AlMg0.5Si; Aluminium 6063-T6; AA6063-T6
Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Vickers
- Ultimate Tensile Strength
- Tensile Yield Strength
- Elongation at Break
- Modulus of Elasticity
- Ultimate Bearing Strength
- Bearing Yield Strength
- Poissons Ratio
- Fatigue Strength
- Machinability
- Shear Modulus
- Shear Strength
- Electrical Resistivity
- CTE, linear 68°F
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Annealing Temperature
- Solution Temperature
- Aging Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|