Aluminum 6262-T8
Subcategory: Aluminum Alloy; Nonferrous Metal; 6000 Series Aluminum Alloy
Close Analogs: Composition Notes: Aluminum content reported is calculated as remainder. Composition information provided by the Aluminum Association and is not for design.
Key Words: Aluminium 6262-T8; UNS A96262; ISO AlMg1SiPb; AA6262-T8
Material Notes: Weldability = B; Stress Corrosion Cracking Resistance = A; General Corrosion Resistance = B (A = best; E = worst). General 6262 characteristics and uses): Good machinability and high strength; high corrosion resistance and applied coating acceptance. Finishing characteristics better than 2011, 2017, 2024, 7075 and equal to 6061. The T8 temper offers excellent residual stress control. Uses: Camera parts, couplings, marine fittings, decorative and misc. hardware, hinge pins, knobs, magneto parts, nuts, oil line fittings, appliance fittings, roller skate parts, steam iron parts, TV fittings, tripod fittings, valves and valve parts. Some data provided by Alcoa. Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell A
- Hardness, Rockwell B
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Machinability
- Shear Modulus
- Shear Strength
- Electrical Resistivity
- CTE, linear 68°F
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Annealing Temperature
- Solution Temperature
- Aging Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|