Aluminum 8030-H221
Subcategory: Aluminum Alloy; Nonferrous Metal; Other Wrought Al Alloy
Close Analogs: Composition Notes: Aluminum content reported is calculated as remainder. Composition information provided by the Aluminum Association and is not for design.
Key Words: Aluminium 8030-H221; AA8030-H221
Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.
| Available Properties |
- Density
- Electrical Resistivity
- CTE, linear 68°F
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|