Aluminum 8090-T852
Subcategory: Aluminum Alloy; Nonferrous Metal; Other Wrought Al Alloy
Close Analogs: Composition Notes: Aluminum content reported is calculated as remainder. Composition information provided by the Aluminum Association and is not for design.
Key Words: Aluminium 8090-T852; AlLi; Aluminum Lithium Alloy; AA8090-T852; UNS A98090
Material Notes: Common heat treatment for die forgings with cold work and hand forgings. Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell A
- Hardness, Rockwell B
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Fracture Toughness
- Shear Strength
- CTE, linear 20°C
- Specific Heat Capacity at Elevated Temperature
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|