Aluminum 8090-T8771 and 8090-T651
Subcategory: Aluminum Alloy; Nonferrous Metal; Other Wrought Al Alloy
Close Analogs: Composition Notes: Aluminum content reported is calculated as remainder. Composition information provided by the Aluminum Association and is not for design.
Key Words: AA8090-T8771; AA8090-T651; UNS A98090, Aluminium 8090-T8771; Aluminium 8090-T651; AlLi; Aluminum Lithium Alloy
Material Notes: Peak aged. Common heat treatment for medium-strength plate. Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell A
- Hardness, Rockwell B
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Fracture Toughness
- Shear Strength
- CTE, linear 20°C
- Specific Heat Capacity at Elevated Temperature
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|