Aluminum 355.0-T62, Permanent Mold Cast
Subcategory: Aluminum Alloy; Nonferrous Metal; Aluminum Casting Alloy
Close Analogs: Composition Notes: If iron exceeds 0.45%, manganese content shall not be less than one-half iron content. Aluminum content reported is calculated as remainder. Composition information provided by the Aluminum Association and is not for design.
Key Words: Aluminium 355.0-T62; UNS A03550; ISO 3522: AlSi5Cu1Mg; ISO R164: AlSi5Cu1; AA355.0-T62
Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell A
- Hardness, Rockwell B
- Hardness, Vickers
- Ultimate Tensile Strength
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Compressive Yield Strength
- Poissons Ratio
- Fatigue Strength
- Machinability
- Shear Modulus
- Shear Strength
- Electrical Resistivity
- Heat of Fusion
- CTE, linear 68°F
- CTE, linear, 482°F (250°C)
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Melt Temperature
- Solution Temperature
- Aging Temperature
- Casting Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|