Aluminum B357.2 Composition Spec
Subcategory: Aluminum Alloy; Nonferrous Metal; Aluminum Casting Alloy
Close Analogs: Composition Notes: Aluminum content reported is calculated as remainder. Composition information provided by the Aluminum Association and is not for design.
Key Words: Aluminium B357.2; AAB357.2
Material Notes: This data sheet has no physical/mechanical property data. Most MatWeb aluminum entries, especially entries with a specific temper in the name, have much more property data.