Aluminum 413.0-F Die Casting Alloy
Subcategory: Aluminum Alloy; Nonferrous Metal; Aluminum Casting Alloy
Close Analogs: Composition Notes: Aluminum content reported is calculated as remainder. Composition information provided by the Aluminum Association and is not for design.
Key Words: Aluminium 413.0-F; UNS A04130; AA413.0-F Die, ISO 3522 AlSi12CuFe and AlSi12Fe. ISO R164 AlSi12, AlSi12Cu, AlSi12CuFe, AlSi12Fe. ISO R2147 AlSi12, EN 1706 AC 44100, BB401, CC401, EA401, G-AlSi12, DIN 230, UNI 4514, AS 13, RSA SA 22
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Fatigue Strength
- Machinability
- Shear Strength
- Electrical Resistivity
- Heat of Fusion
- CTE, linear 20°C
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Melt Temperature
- Casting Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|