High-Nickel Ductile Iron, corrosion resistant
Subcategory: Ductile Iron; Alloy Cast Iron; Metal
Close Analogs: Ni-Resist austenitic iron, ASTM A439
Key Words: Corrosion resistant high-nickel ductile iron, ASTM A439, austenitic
Material Notes: Austenite matrix structure as cast.
| Available Properties |
- Density
- Electrical Resistivity
- CTE, linear 20°C
- Thermal Conductivity
|
|
|
|