High-Nickel Ductile Iron, heat-resistant ductile iron, 23% Ni
Subcategory: Ductile Iron; Alloy Cast Iron; Metal
Close Analogs: Ni-Resist austenitic iron, ASTM A439
Key Words: 23% Ni heat-resistant ductile iron high-nickel ductile iron , austenitic
Material Notes: Austenite matrix structure as cast.
| Available Properties |
- Density
- Electrical Resistivity
- CTE, linear 20°C
|
|
|
|