Aluminum LM2 As Manufactured, Gravity Die Cast
Subcategory: Aluminum Alloy; Aluminum Casting Alloy
Key Words: Al Si10 Cu2, BS 1490, LM 2; Aluminium
Material Notes: Description: LM2 is an aluminum casting alloy with fair durabiliy, good corrosion resistance, and average strength. It is a good choice for most die cast applications that do not require high corrosion (marine appliations). This grade has a dark grey color after anodizing. Applications: cast rainwater goods Aluminum calculated as remainder. One other form of this alloy is in the database.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Elongation at Break
|
|
|
|
| Property Data |