|   Aluminum LM2 As Manufactured, Pressure Die Cast  Subcategory: Aluminum Alloy; Aluminum Casting Alloy Key Words: Al Si10 Cu2, BS 1490, LM 2; Aluminium Material Notes: Description:  LM2 is an aluminum casting alloy with fair durabiliy, good corrosion resistance, and average strength. It is a good choice for most die cast applications that do not require high corrosion (marine appliations). This grade has a dark grey color after anodizing.
 Applications: cast rainwater goods Aluminum calculated as remainder. One other form of this alloy is in the database. 
| | 