|   Aluminum LM4 As Manufactured, Sand Cast  Subcategory: Aluminum Alloy; Aluminum Casting Alloy Key Words: Al Si5 Cu3, BS 1490, LM 4; Aluminium Material Notes: Description: LM4 is fairly durable and, with treatment, is moderately strong. It is very versatile but is rarely pressure die cast.
 Applications: sections that require pressure tightness, castings, and handles. . Aluminum calculated as remainder. Three other forms of this alloy are in the database. 
| | 
    | Available Properties |  
    | DensityTensile Strength, UltimateElongation at Break
 | 
 | 
 |  | | 
    | Property Data |  
    | 