Aluminum LM6 As Manufactured, Gravity Die Cast
Subcategory: Aluminum Alloy; Aluminum Casting Alloy
Key Words: Al Si12, BS 1490, LM 6; Aluminium
Material Notes: Description: LM6 is a corrosion resistant aluminum casting alloy with average durability and strength, and with high impact strength and ductility.Applications: general, electrical, marine, intricate shaped castings, and building cladding panels Aluminum calculated as remainder. One other form of this alloy is in the database.