|   Class II Type E 20% Cr-Mo-HC Martensitic White Cast Iron  Subcategory: White Cast Iron; High Carbon Steel; Metal Key Words: Class II Type E 20% Cr-Mo-HC martensitic white cast iron, ASTM A532-75a Material Notes: Standard martensitic white cast iron from ASTM A532-75a. 300 mm typical maximum section thickness.
 
| | 
    | Available Properties |  
    | DensityHardness, BrinellHardness, KnoopHardness, Rockwell CHardness, Vickers
 | 
 | 
 |  | | 
    | Property Data |  
    | 