ASTM A516, Grade 60
Subcategory: Low Carbon Steel; Metal; Pressure Vessel Steel; Nonresulfurized Steel
Material Notes: For moderate and lower temperature serice. Maximum plate thickness is only limited by the capacity of the composition to meet the specified mechanical property requirements; however, current production of ASTM A516 Grade 60 plates are normally limited to maximum thickness of 8 in. (205 mm).
| Available Properties |
- Density
- Tensile Strength, Yield
- Elongation at Break
|
|
|
|
| Property Data |