Beryllium PR-200; 0.45 - 0.60 inch thick sheet

 

Subcategory: Pure Element; Nonferrous Metal; Beryllium Alloy

Key Words: Brush Wellman; PR200 Alloys

Material Notes:
Composition above is reported for product available from Brush Wellman. Tensile data below for this thickness PR-200 has been supplemented with other property data generally applicable to pure beryllium.

Manufactured by warm-rolling billets of vacuum hot pressed block encased in steel. Rolling creates anisotropy in the product, so cross-directional rolling techniques are often used.

Please note that there are health hazards associated with beryllium, especially when present as airborne particles generated during processing. As with any material, be aware of hazards and take steps to reduce exposure to a safe level.

General beryllium information: Beryllium is one of the lightest metals and has a high strength-to-weight ratio, stiffness-to-weight ratio, and very high specific heat, thermal conductivity, and heat of fusion. It has significant ductility, is readily machined and can be rolled, drawn, or extruded. It finds applications in nuclear reactors (neutron moderator and reflector), X-ray sources/detectors (X-ray transparency), IR target acquisition systems, inertial guidance instruments, computer parts, other aircraft and satellite structures, and heat sink constraining cores. Beryllium is usually produced via a powder metallurgy process to improve machinability and mechanical properties.

Information provided by Brush Wellman and the references.

Available Properties
  • Density
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Poissons Ratio
  • Shear Modulus
  • Electrical Resistivity
  • Magnetic Susceptibility
  • Critical Superconducting Temperature
  • Heat of Fusion
  • CTE, linear 20°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • CTE, linear 1000°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Emissivity (0-1)
  • Reflection Coefficient, Visible (0-1)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。