Oxygen-free electronic Copper, UNS C10100
Subcategory: Copper Alloy; Nonferrous Metal; Wrought Copper
Close Analogs: UNS C10100 - ASTM (flat products) B48, B133, B152, B187, B272, B432, B451, F68, (pipe) B42, B188, F68, (rod) B12, B49,B133, B187, F68, (shapes) B113, B187, F68, (tubing) B372, B68, B75, B188, B280, F68, (wire) B1, B2, B3, F68 ; 101A (Australia); C110 (UK); CDA 101 OFE; ISO Cu-OFE, JIS C1011 H3510 (Japan)
Key Words: ISO Cu-FRTP, CEN CW006A, C110, ISO Cu-OFE, CEN CW009A, certified OFHC, high conductivity copper, QQ-C-502, CDA 101 OFE, JIS C1011 H3510
Material Notes: Applications: busbars, bus conductors, waveguides, hollow conductors, lead-in wires and anodes for vacuum tubes, vacuum seals, transistor components, glass to metal seals, coaxial cables, klystrons, microwave tubes, and rectifiers. Processing: Excellent hot and cold workability; good forgeability. Fabricated by bending, coining, coppersmithing, drawing and upsetting, hot forging and pressing, knurling, roll threading, shearing, spinning, swaging, and stamping. Corrosion Resistance: Good to excellent. Susceptible to galvanic corrosion when coupled with iron, aluminum, magnesium, lead, tin, and zinc. Good resistance to atmospheric, brackish water, sea water, and non-oxidizing acid corrosion, but avoid heating in oxidizing atmospheres or exposing to oxidizing acids, moist halogens, sulfides, ammonia, or solutions with ammonium ions. Forms: pipe, plate, rod, shapes, sheet, strip, tube, and wire.
| Available Properties |
- Density
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 100°C
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|