|   Oxygen-free high conductivity Copper, Soft, UNS C10200  Subcategory: Copper Alloy; Nonferrous Metal; Wrought Copper Close Analogs: UNS C10200 - ASTM (flat products) B48, B133, B152, B187, B272, B370, B432, B451, (pipe) B42, B188, (rod) B12, B49, B124,B133, B187, (tubing) B68, B75, B88, B111, B188, B280, B359, B372, B395, B447, (shapes) B124,B133, B187, (wire) B1, B2, B3, B33, B47, B116, B189, B246, B286, B298, B355; C103 (UK); CDA 102 OF; CEN CW009A; Cu/cl NF A53301 (France), ISO Cu-OF R1337; JIS C1020 H3100 - sheet, plate, C1020 H3140 - bar (Japan); QQ-C-576 (flat products), QQ-C-502 (rod, shapes); QQ-C-576 (tube); QQ-C-502, QQ-W-343, MIL-W-3318 (wire) Key Words: AS 101A 1567 (Australia), OFHC, coining, coppersmithing, ASTM B1, B2, B3, B12, B33, B42, B47, B48, B49, B68, B75, B88, B111, B116, B124, B133, B152, B187, B188, B189, B246, B272, ASTM B286, B298, B355, B359, B370, B372, B395, B432, B451, B447, C103, CDA 102 OF, CEN CW009A, Cu/cl NF A53301, QQ-C-576, CDA 102 OF, C103, ISO Cu-OF R1337, CEN CW008A, OFHC Material Notes: UNS C10200 contains a minimum of 99.95 Cu+AgApplications: busbars, bus conductors, waveguides, hollow conductors, lead-in wires and anodes for vacuum tubes, vacuum seals, transistor components, glass to metal seals, coaxial cables, klystrons, microwave tubes, and rectifiers.
 Processing: Excellent hot and cold workability; good forgeability. Fabricated by bending, coining, coppersmithing, drawing and upsetting, hot forging and pressing, knurling, roll threading, shearing, spinning, swaging, and stamping. Corrosion Resistance: Good to excellent.  Susceptible to galvanic corrosion when coupled with iron, aluminum, magnesium, lead, tin, and zinc.  Good resistance to atmospheric, brackish water, sea water, and non-oxidizing acid corrosion, but avoid heating in oxidizing atmospheres or exposing to oxidizing acids, moist halogens, sulfides, ammonia, or solutions with ammonium ions. Forms: pipe, plate, rod, shapes, sheet, strip, tube, and wire. 
| | 
    | Available Properties |  
    | DensityHardness, VickersTensile Strength, UltimateTensile Strength, YieldElongation at BreakModulus of ElasticityPoissons RatioIzod ImpactFatigue StrengthMachinabilityShear ModulusElectrical ResistivityCTE, linear 20°CCTE, linear 100°CCTE, linear 250°CSpecific Heat CapacityThermal ConductivityMelting Point
 | 
 | 
 |  | | 
    | Property Data |  
    | 
    This page displays only the textof a material data sheet.
 
 To see MatWeb's complete data
 sheet for this material (including
 material property data, metal
 compositions, material suppliers,
 etc), please click the button below.
 |  
    |  | 
 | 
 | 
 |