Oxygen-free Copper (OF), UNS C10200, H02 Temper, flat products

 

Subcategory: Copper Alloy; Nonferrous Metal; Wrought Copper

Close Analogs: UNS C10200 - ASTM B48, B133, B152, B187, B272, B370, B432; C103 (UK); CDA 102 OF; CEN CW009A; ISO Cu-OF R1337; JIS C1020 H3100 (sheet, plate) (Japan); QQ-C-576

Key Words: BS C110, C103, ISO Cu-OF R1337, CEN CW009A, oxygen free high conductivity copper (OFHC), CDA 102 OF, ASTM B48, B133, B152, B187, B272, B370, B432, Cu/cl NF A53301, C1020 H3100, C1020 H3140, flat products, plates, sheets, strips, QQ-C-576

Material Notes:
Copper content in composition table includes silver (minimum 99.95% Cu+Ag). Flat test specimen, 1mm thick, H02 temper.

Applications: busbars, bus conductors, waveguides, hollow conductors, lead-in wires and anodes for vacuum tubes, vacuum seals, transistor components, glass-to-metal seals, coaxial cables, klystrons, microwave tubes, and rectifiers.

Processing: Excellent hot and cold workability; good forgeability. Fabricated by bending, coining, coppersmithing, drawing and upsetting, hot forging and pressing, knurling, roll threading, shearing, spinning, swaging, and stamping.

Corrosion Resistance: Good to excellent. Susceptible to galvanic corrosion when coupled with iron, aluminum, magnesium, lead, tin, and zinc. Good resistance to atmospheric, brackish water, sea water, and non-oxidizing acid corrosion, but avoid heating in oxidizing atmospheres or exposing to oxidizing acids, moist halogens, sulfides, ammonia, or solutions with ammonium ions.

Available Properties
  • Density
  • Hardness, Rockwell B
  • Hardness, Rockwell F
  • Hardness, HR30T
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Poissons Ratio
  • Fatigue Strength
  • Machinability
  • Shear Modulus
  • Shear Strength
  • Electrical Resistivity
  • CTE, linear 20°C
  • CTE, linear 100°C
  • CTE, linear 250°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Annealing Temperature
  • Hot-Working Temperature
  • Recrystallization Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。