Oxygen-free Copper (OF), UNS C10200, H55 (15%) temper, tubing
Subcategory: Copper Alloy; Nonferrous Metal; Wrought Copper
Close Analogs: UNS C10200 - ASTM B68, B75, B88, B111, B188, B280, B359, B372, B395, B477; C103 (UK); CDA 102 OF; CEN CW009A; ISO Cu-OF R1337;JIS C1020 (Japan); QQ-C-576
Key Words: ASTM B68, B75, B88, B111, B188, B280, B359, B372, B395, B477, BS C110, C103, ISO Cu-OF R1337, CEN CW009A, oxygen free high conductivity copper (OFHC), CDA 102 OF, tubes, tubing, CDA 102 OF, WW-T-775
Material Notes: Copper content in composition table includes silver (minimum 99.95% Cu+Ag). Test specimen: tubing, 25mm diam., 1.65 mm wall thickness. Applications: busbars, bus conductors, waveguides, hollow conductors, lead-in wires and anodes for vacuum tubes, vacuum seals, transistor components, glass-to-metal seals, coaxial cables, klystrons, microwave tubes, and rectifiers. Processing: Excellent hot and cold workability; good forgeability. Fabricated by bending, coining, coppersmithing, drawing and upsetting, hot forging and pressing, knurling, roll threading, shearing, spinning, swaging, and stamping. Corrosion Resistance: Good to excellent. Susceptible to galvanic corrosion when coupled with iron, aluminum, magnesium, lead, tin, and zinc. Good resistance to atmospheric, brackish water, sea water, and non-oxidizing acid corrosion, but avoid heating in oxidizing atmospheres or exposing to oxidizing acids, moist halogens, sulfides, ammonia, or solutions with ammonium ions.
| Available Properties |
- Density
- Hardness, Rockwell B
- Hardness, Rockwell F
- Hardness, HR30T
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Machinability
- Shear Modulus
- Shear Strength
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 100°C
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Annealing Temperature
- Hot-Working Temperature
- Recrystallization Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|