Oxygen-free extra-low phosphorus Copper, UNS C10300, OS050 temper, flat products, tube, and shapes
Subcategory: Copper Alloy; Nonferrous Metal; Wrought Copper
Close Analogs: UNS C10300, CDA 103, ASTM (flat products) B133, B152, B187, B272, B432, (tubing) B68, B75, B88, B111, B188, B251, B280, B306, B359, B372, B395, B447, (shapes) B133, B187
Key Words: OFXLP, ASTM B280, 306, 359, 372, 395, 432, 447, CDA 103, ASTM B68, 75, 88, 111, 133, 152, 187, 188, 251, 272
Material Notes: Note: Cu percentage includes Cu+Ag+P. Test specimens: flat products - 1 mm and 6 mm thick; tube - 25 mm OD, 1.65 mm thick; shape - 13 mm section. Applications: electrical conductors and terminals, tubular busbars, commutators, copper clad steel and clad products, waveguide tubing, thermostatic control tubing, and applications requiring good conductivity and welding or brazing properties. Processing: Excellent hot and cold workability; good forgeability. Annealing temp.: 475-750°C (900-1400°F). Hot working temp.: 750-875°C (1400-1600°F). Fabricated by coining, coppersmithing, drawing and upsetting, hot forging and pressing, spinning, swaging, stamping. Corrosion Resistance: Good to excellent Weldability: excellent welding and brazing properties.
| Available Properties |
- Density
- Hardness, Rockwell F
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Machinability
- Shear Modulus
- Shear Strength
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 100°C
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|