SAE J431 automotive gray cast iron, SAE grade G3000
Subcategory: Gray Cast Iron; Metal
Key Words: UNS F10006, ferritic, pearlitic, soft iron castings
Material Notes: If Carbon or Silicon is on the high % range end, the other should be on the low % end. Properties determined from as-cast test bar 30.5 mm diameter. Pearlitic microstructure. Applications include automobile and diesel cylinder blocks, cylinder heads, flywheels, differential carrier castings, pistons, medium duty brake drums and clutch plates. 1000 kg minimum transverse load, 5.1 mm minimum deflection.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
|
|
|
|