SAE J431 automotive gray cast iron, SAE grade G3500
Subcategory: Gray Cast Iron; Metal
Key Words: UNS F10007, ferritic, pearlitic, soft iron castings
Material Notes: If Carbon or Silicon is on the high % range end, the other should be on the low % end. Properties determined from as-cast test bar 30.5 mm diameter. Pearlitic microstructure. Applications include diesel engine blocks, truck and tractor cylinder blocks and heads, heavy flywheels, tractor transmission cases, heavy gear boxes. 1110 kg minimum transverse load, 6.1 mm minimum deflection.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
|
|
|
|
| Property Data |